#1
|
||||
|
||||
They need to put it back in the ocean...
This was on a local buyselltrade group for $250. No, I'm not interested, just curious what caused the severe "pitting". Looks like they were using it for a boat mooring...
__________________
TA Arcmaster 185 w/tig/stick kit MillerMatic 252 w/3rd gen 30A MM140 w/o AS, w/CO2 Hobart (Miller) 625 plasma Hobart 250ci plasma Victor O/A (always ready, but bored) HF 80 lunchbox w/tig 45ACP Black Talons for those stubborn jobs... |
#2
|
||||
|
||||
Yeah laying on the bottom of something in salt water. Also if it was at the bottom of a pile of scrap, with some aluminum, galvanic corrosion for many years.
it is just scrap a this point.
__________________
Shade "Prepare to defend yourselves." -- Sergeant Major Basil L. Plumley, Ia Drang Valley |
#3
|
||||
|
||||
The top may be a second piece, perhaps it could be replaced. However if I remember right, it’s a tricky process at the best of times to put a face on an anvil.
Sent from my iPhone using Tapatalk |
#4
|
|||
|
|||
At this point, it's best and highest use is attached to the legs of a deserving politician before they go for a swim.
|